Please enjoy the website from a desktop for now.
The OCS Full Notch Creep Test (FNCT) is a widely used method of classifying polyethylene materials in terms of their slow crack growth behaviour under accelerated conditions. A circumferentially notched body is loaded in a tempered wetting agent with a defined tensile stress, and the time until a break occurs is measured.
Tensile force range (infinitely variable pull arm system with 115–315 N) | 2.5–6.5 MPa for samples 10 × 10 × 100 mm with notch depth of 1.6 mm |
Tensile force range (infinitely variable pull arm system with 115–315 N) | 15–40 MPa for samples 6 × 6 × 90 mm with notch depth of 1.6 mm |
Force measurement | Electronic force sensor with a resolution of 0.01 N |
Fluid volume | Approx. 55 l |
Level control | Stainless steel float sensors and magnetic valves |
Inlet pressure range for the supply of demineralised water | 0.2–8 bar (3–116 psi) |
Communication protocol | MODBUS (RTU, TCP/IP), PROFIBUS, PROFINET, OPC (Server/Client), CSV file, customer-specific |